Laser ablation plume while depositing a YBa2Cu3O7
thin-film.

Barrel chamber for oxygen plasma treatment of YBa2Cu3O7 thin-films.

A multiloop dc SQUID from 2 YBa2Cu3O7 layers and
an intermediate SrTiO3 insulation layer. The diameter is 7 mm.
The smallest structures on this chip are 3 µm wide.
The measurement setup:
- Multimeter,
- SQUID FLL electronics,
- Temperature controller,
- Waveform generator,
- Oscilloscope,
- FFT signal analyzer,
- Lock-in amplifier,
- Multi purpose data acquisition unit,
- Lead acid battery chargers,
- Battery powered modular SQUID electronics,
- Probe holder,
- Apple Power Macintosh,
- Liquid nitrogen dewar.